Deskripsi
Specifications:
Typical Chemical Composition:
-
Cu: 81-85%
-
Sn: 6.5-7.5%
-
Pb: 6-8%
-
Ni: 1% max
Typical Mechanical Properties:
-
Tensile Strength: 240 MPa (34800 PSI)
-
Yield Strength: 125 MPa (18100 PSI)
-
Elongation: 20%
-
Elastic Modulus: 117 GPa (16969 KSI)
-
Hardness: 65
-
Fatigue Strength: 110 MPa (16000 KSI)
-
Machinability: 70
Applications:
-
Lead is added to improve machinability and pressure tightness
-
Suitable for pump, valve components, general utility bearings, bushings
Profiles Available:
-
Round Bar / Rod
-
Flat Bar
-
Bush / Hollow
-
Sheet / Plate