Soldering Tin Typical Chemical Composition:
-
Lead (Pb): 55%
-
Tin (Sn): 45%
Typical Mechanical Properties:
-
Tensile Strength: 37-41 MPa
-
Elongation: 25-35%
-
Modulus of Elasticity: 23.7-26.9 GPa
-
Shear Strength: 32-36 MPa
Applications:
Zinc Anode Typical Chemical Composition:
-
Iron (Fe): 0.005 max %
-
Cadmium (Cd): 0.025~0.07%
-
Copper (Cu): 0.005 max %
-
Aluminium (Al): 0.10~0.50%
-
Lead (Pb): 0.006 max %
-
Others: 0.10 max %
-
Zinc (Zn): remainder
Applications:
-
Sacrificial Protection.
-
To protect submerged or buried metal structures from corrosion.